Is film-faced plywood waterproof?
No, film-faced plywood is water-resistant rather than waterproof. The phenolic film keeps water and cement paste off the face, and the WBP glue line holds the plies through repeated pours and wet weather, which is the duty the panel is built for. Cut edges and drilled holes expose bare veneer, so they need sealing before the first pour or the core will take on water between cycles. Marine plywood is not waterproof either; permanent immersion is a different job from a pour panel, and even a marine sheet needs coating if it will stay wet.
Can marine plywood be used for concrete forms?
You can pour against it, but it is rarely the right buy. Without a film face, wet concrete grips the bare veneer, stripping scars both the sheet and the wall, and the wood grain prints into the concrete. Marine plywood also costs more at the same thickness and wears out faster on a pour cycle than a film-faced sheet built for that work. If a project needs both products, list them as separate order lines.
Which is cheaper, film-faced or marine plywood?
Film-faced plywood is usually cheaper per sheet at the same thickness. Marine plywood costs more because every ply is selected for a void-free core that can stay wet for years. On a formwork job the fairer comparison is cost per pour, and a film-faced panel that is stripped on time and stored flat wins that comparison.
What is the difference between formply and marine ply in Australia?
Formply is the Australian name for film-faced formwork plywood, and it is stress-graded under AS 6669, most often to F17. Marine ply answers to a different standard, AS/NZS 2272, which looks at core quality and the glue bond rather than pour performance. When comparing formply offers, the useful checks are the F-grade and the film, plus the reuse rating, rather than the name on the sheet.
Which bond class do Vinawood's film-faced and marine grades meet?
Eco Form Plus and Form Basic are EN 636-2 Class 2 panels for humid conditions and standard formwork, and Form Extra uses a more durable MUF glue (WBP Melamine Top) in the same class, rated for up to 15 reuses. Pro Form Lite, Pro Form, HDO Standard and HDO Premium use phenolic glue and meet EN 636-3 Class 3, while HDO Basic sits in Class 2. Marine Standard and Marine Extra are bonded with WBP Melamine Top glue rated EN 636-2, so a boat or dock specification that calls for phenolic glue should state that requirement on the RFQ. If the engineer writes Class 3, a Class 2 grade should not be swapped in.
What does "film faced marine plywood" mean on a trading list?
Trading lists that use the label "film faced marine plywood" usually describe a film-faced formwork panel with a WBP glue line, and the word "marine" is there to signal water resistance rather than a BS 1088 core. The label alone does not make the sheet a void-free marine panel. Ask for the core grade and the EN 636 class in writing before you compare prices.